Self-inspection by pickling workers is a critical step in quality control for their steel pipes. Only through collective quality management can we ensure minimal or no defective products. Therefore, pickling workers must inspect the following aspects: whether the steel pipe surface shows signs of over-pickling, under-pickling, wire sticking, oil stains, paint scars, bubbles, dirt adhering to the base pipe surface, or the presence of harmful elements such as pickling sludge and iron salts that may affect hot-dip galvanizing. If any of these issues are detected, appropriate corrective measures should be implemented.
46. What aspects are covered in the self-inspection process for pickling?
Dec 30, 2025
Send Inquiry
Related Knowledge
-
86. What impact does pre-treatment have on the adhesion of the galvanized layer?18 Mar, 2026 -
85. What is the effect of molten zinc temperature on zinc slag? At what iron content in molten zi...18 Mar, 2026 -
84. How does zinc slag affect the galvanized coating of galvanized steel pipes?16 Mar, 2026 -
83. How is zinc slag formed? What are its components?16 Mar, 2026